摩托车前大灯线夹断裂工艺分析
引用本文:王峥琎.摩托车前大灯线夹断裂工艺分析[J].摩托车技术,2006(4):26-28.
作者姓名:王峥琎
作者单位:江苏省盐城市圣茂机械厂
摘    要:线夹凹凸面折弯处圆角过小引起应力集中,是造成前大灯线央断裂的主要原因。加上电镀后未采取去氢脆处理、热处理温度不稳定超过上限值等原因,致使前大灯线夹在安装和维修保养时从3.5 mm开口处张开造成断裂。

关 键 词:弹性薄壁  前大灯线夹  工艺分析
收稿时间:2006-03-07
修稿时间:2006年3月7日

An Analysis of Manufacturability of Thin-walled Parts
Wang Zhengjin.An Analysis of Manufacturability of Thin-walled Parts[J].Motorcycle Technology,2006(4):26-28.
Authors:Wang Zhengjin
Institution:Jiangsu Yancheng Shengmao Machinery Factory
Abstract:The stress concentration caused by the too-small fillet at the area where the male-and-female face of the terminal holder bends is the main reason breaking the headlamp terminal holder. What' s more, the following factors, such as, no hydrogen brittleness treating after painted, the unstable temperature for heat treatment which surpasses the upper limit, etc. worsen the case.
Keywords:Elastic thin-wall Headlamp terminal holder Technological analysis